MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Calcium Carbonate (CaCO3) Filler

Material Notes: Information provided by A.D. Compound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Filler Content 40 %ISO 3451 / 1
Melt Index of Compound 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ISO 868
Tensile Strength, Yield 20.0 MPaISO 527
Elongation at Break 50 %ISO 527
Elongation at Yield 8.0 %ISO 527
Flexural Modulus 1.80 GPaISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²ISO 180/1U
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CISO 75
Vicat Softening Point 76.0 °C49 N; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman LPP40YR04BK 40% Calcium Carbonate Filled, Copolymer Polypropylene
Washington Penn Homopolymer Polypropylene 40% Calcium Carbonate Filled
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
LATI Latene® 3 CA/40 40% Calcium Carbonate Polypropylene Homopolymer (PPH)
Albis Plastics Polypropylene PP 14A10 CaCO3 40 , 40% Calcium Carbonate (CaCO3)

PADCOM13 / 22591

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.