MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior ForTii® F12 PPA-GF40 FR(40) PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® F12 has excellent balance of stiffness and toughness, suitable for high mechanical loaded application such as power connector or EV parts. F12 has high RTI electrical rating of 140°C at 0.75 mm and shows JEDEC Level 2 performance, enabling SMT process without deformation and low risk on blistering.

Features: Phosphorous free. 40% glass reinforced. Processing: Injection Molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccDry; ISO 1183
Moisture Absorption 1.30 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0085 cm/cmDry; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPaDry; ISO 527-1/-2
 170 MPaCond; ISO 527-1/-2
Elongation at Break 1.9 %Dry; ISO 527-1/-2
 1.9 %Cond; ISO 527-1/-2
Tensile Modulus 13500 MPaDry; ISO 527-1/-2
 13500 MPaCond; ISO 527-1/-2
Flexural Strength 260 MPaCond; ISO 178
 280 MPaDry; ISO 178
Flexural Modulus 14500 MPaDry; ISO 178
 14500 MPaCond; ISO 178
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 65.0 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
Dry; IEC 60250
 3.9
@Frequency 1e+6 Hz
Cond; IEC 60250
 4.2
@Frequency 100 Hz
Dry; IEC 60250
 4.2
@Frequency 100 Hz
Cond; IEC 60250
Dielectric Strength 33.0 kV/mmDry; IEC 60243-1
 33.0 kV/mmCond; IEC 60243-1
Comparative Tracking Index 600 VDry; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°CASTM D696
CTE, linear, Parallel to Flow 30.0 µm/m-°CASTM D696
Melting Point 325 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 305 °CDry; ISO 75-1/-2
UL RTI, Electrical 140 °C
@Thickness 0.350 mm
UL746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7904 / 291340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.