MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Texin® 4215 Thermoplastic Polyurethanes (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: Texin 4215 resin is a blend of polyester-based polyurethane and polycarbonate. This aromatic grade has a Shore hardness of approximately 75D*. It can be processed by injection molding or extrusion.

Properties / Applications: Texin 4215 resin offers high impact strength, and high stiffness, as well as excellent low-temperature properties. Typical applications include automotive cladding, fascia, bumpers, and a wide variety of injection molded and extruded articles. As with any product, use of Texin 4215 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength at Break 45.5 MPaASTM D412
Elongation at Break 130 %ASTM D412
Flexural Modulus 1100 MPaASTM D790
Compressive Strength 3.40 MPa2% Deflection; ASTM D 575
 13.8 MPa5% Deflection; ASTM D 575
Resilience 52[%], Bayshore; ASTM D2632
Izod Impact, Notched 1.50 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 18.0 ft-lb/in
@Temperature 23.0 °C
ASTM D256
Tear Strength 167 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 85
@Load 1.00 kg
[mg] Loss, H-18; ASTM D3489
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 108 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CASTM D648
Vicat Softening Point 140 °CRate A; ASTM D1525
Brittleness Temperature >= -68.0 °FASTM D746
Glass Transition Temp, Tg -35.0 °C
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 221 - 232 °CInjection
Middle Barrel Temperature 227 - 238 °CInjection
Front Barrel Temperature 227 - 238 °CInjection
Nozzle Temperature 227 - 241 °CInjection
Zone 1 210 - 227 °CExtrusion
Zone 2 216 - 232 °CExtrusion
Zone 3 216 - 238 °CExtrusion
Die Temperature 221 - 243 °CExtrusion
Melt Temperature 232 - 238 °CInjection
 232 - 243 °CExtrusion
Mold Temperature 16.0 - 43.0 °CInjection
Injection Pressure 6000 - 15000 psiInjection
Hold Pressure 4000 - 8000 psiInjection
Back Pressure 50.0 - 200 psiInjection
Cushion <= 0.125 inInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2558 Polycarbonate
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU)
Covestro Texin® 4210 Thermoplastic Polyurethanes (TPU)
Covestro Texin® STX Thermoplastic Polyurethanes (TPU)
Covestro Texin® 985 U Thermoplastic Polyurethanes (TPU)

PCOVEST0992 / 202775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.