MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium AM50A-F, Die Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Excellent energy-absorption characteristics and excellent ductility. Applications for die casting alloy in as-cast (F) temper include parts that require good ductility and toughness with reasonable yield and tensile properties (such as automotive wheels).

Key Words: UNS M10500; ASTM B 94; European EN 1753 MC21220 (Ingot UNS M10501)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 60500 kg load, 10 mm ball
Tensile Strength, Ultimate 33000 psi
Tensile Strength, Yield 18000 psi
Elongation at Break 15 %in 50 mm
Modulus of Elasticity 45.0 GPa
Compressive Yield Strength 16000 psi
Poissons Ratio 0.35
Shear Modulus 17.0 GPaEstimated from similar Mg alloys.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000130 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 µm/m-°C
@Temperature 20.0 - 100 °C
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.02 J/g-°C
Thermal Conductivity 65.0 W/m-K
Melting Point >= 435 °CIncipient Melting
Liquidus 620 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 655 - 690 °CDie Cast
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.4 - 5.4 %
Copper, Cu <= 0.010 %
Iron, Fe <= 0.0040 %
Magnesium, Mg 94.8 %As Remainder
Manganese, Mn 0.26 - 0.60 %
Nickel, Ni <= 0.0020 %
Other, each <= 0.020 %
Silicon, Si <= 0.10 %
Zinc, Zn <= 0.22 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AM60A-F, Die Cast
Magnesium AZ91D-F, Cast
Magnesium AM60B-F, Die Cast
Magnesium AM20-F, Die Cast
Magnesium AM100A-T4, Cast

MMAM50AF / 12298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.