MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-555 Thermoplastic Elastomer, Medical Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-555 is a high performance thermoplastic elastomer intended for use in healthcare and medical applications. Medalist MD-555 is a medium hardness, low density, clear grade designed to be a sustainable alternative to flexible PVC with excellent processability and throughput in extruded tubing. .

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Processability; Good Sterilizability; Halogen Free; High Clarity; High purity: Low Density; Low Specific Gravity; Medium Hardness; No Animal Derived Components; Radiation (Gamma) Resistant

Uses: Film; Medical/Healthcare Application; Pharmaceutical; Rubber Replacement; Tubing

Form: Pellets

Processing Method: Cast Film; Extrusion; Injection Molding

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 535 seconds; ASTM D2240
 551 seconds; ASTM D2240
Tensile Strength 1340 psiASTM D412
Tensile Stress at Strain 220 psi
@Strain 50 %
ASTM D412
 270 psi
@Strain 100 %
ASTM D412
 415 psi
@Strain 300 %
ASTM D412
Elongation at Break 890 %ASTM D412
Tear Strength 31.0 kN/mASTM D624
Compression Set 9.1 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 280 - 320 °F
Front Barrel Temperature 300 - 340 °F
Nozzle Temperature 340 - 380 °F
Zone 1 340 - 370 °F
Zone 2 360 - 385 °F
Zone 3 365 - 400 °F
Zone 4 365 - 400 °F
Zone 5 400 - 440 °F
Die Temperature 400 - 440 °F
Melt Temperature 340 - 380 °FProcessing Temp
Mold Temperature 70.0 - 100 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-590 Thermoplastic Elastomer, Medical Grade
Teknor Apex Medalist® MD-575 Thermoplastic Elastomer, Medical Grade
Teknor Apex Medalist® MD-585 Thermoplastic Elastomer, Medical Grade
Teknor Apex Medalist® MD-565 Thermoplastic Elastomer, Medical Grade
Teknor Apex Medalist® MD-100 Thermoplastic Elastomer

PTEKNO921 / 129102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.