MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Features

Modified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitable for automotive, engineering, electrical and consumer goods industry. With the increasing content of GF also the toughness, tensile and bending strength, modulus in tension and bending increase and the shrinkage decreases as well as the heat application increases up to 150°C. Additional drying of the material is not necessary. Delivered in natural mode and in the full RAL colour scale. Production of the fuel tank caps for the transport vehicles, shells for the textile industry.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Linear Mold Shrinkage 0.0072 cm/cm
Linear Mold Shrinkage, Transverse 0.0082 cm/cm
Melt Flow 6.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa
Elongation at Break 30 %
Tensile Modulus 5650 MPa
Flexural Strength 128 MPa
Flexural Modulus 4890 MPa
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -20.0 °C
 50.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -20.0 °C
 11.0 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °C
Deflection Temperature at 1.8 MPa (264 psi) 134 °C
Vicat Softening Point 162 °CB
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 80.0 °C
Dry Time 2 hour
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latene® 3 G/30 30% Glass Fiber Reinforced Polypropylene Homopolymer (PPH)
LATI Latene® 3 G/20 20% Glass Fiber Reinforced Polypropylene Homopolymer (PPH)
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled

PPLACO311 / 120935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.