MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sinotek Materials ZSLG95 High Carbon Graphite
Categories: Carbon; Graphite; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: The flake graphite acquires advantages such as: superior crystallization, thin flake, good flexibility, excellent chemical and physical properties, superior conductivity, self-lubricity, and resistance to temperature, corrosion and hot shock. Flake graphite is widely used as an essential nonmetallic in almost all industries. It can be used as high-quality refractory material or coatings in metallurgical industry, black lead in light industry, carbon brush in electronics industry, electrode in battery industry, and catalyst in chemical fertilizer industry. After further processing, crystalline flake graphite can be used to produce TV tube coatings, graphite friction reducing additives and many other high-tech products.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.90 %
Ash <= 4.1 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 95 %
H2O, Water 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek CRB-100 Resin-Impregnated Carbon Graphite
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-1205 Graphite
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating

CSINOT04 / 2061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.