MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Carbon Fiber Composite

Material Notes: CF 9040A is a high strength carbon fiber phenolic molding compound

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 g/ccISO 60
Density 1.45 g/ccISO 1183
Water Absorption 0.90 %ISO 62
Linear Mold Shrinkage 0.0010 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 100ISO 2039/2
Tensile Strength at Break 120 MPaISO 527
Flexural Strength 245 MPaISO 178
Flexural Modulus 23.0 GPaISO 178
Compressive Strength 320 MPaISO 604
Charpy Impact, Notched 2.00 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°CASTM E831
CTE, linear, Transverse to Flow 20.0 µm/m-°CASTM E831
 
Descriptive Properties
ColorBlack
FormPellet
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit Vyntec® CF8050 Carbon Fiber Reinforced Phenolic
Sumitomo Bakelite Vyntec® CF8030 Phenolic Moldable Composite
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
LNP Lexan® EXCP0108 Polycarbonate, 30% Carbon Fiber Reinforced

P90X929 / 142704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.