MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys Minspar™ 200 Feldspar
Categories: Ceramic; Clay; Feldspar Clay; Oxide; Silicon Oxide

Material Notes: Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 44.0 lb/ft³loose
 70.0 lb/ft³packed
Brightness 94 %Dry Brightness (Green Filter)
Particle Size 5.0 µm19% finer than
 10 µm40% finer than
 12 µmmean
 20 µm72% finer than
 30 µm87% finer than
Particle Mesh Size 20 Mesh0% retained
 30 Mesh0% retained
 40 Mesh0% retained
 100 Meshtrace retained
 140 Meshtrace retained
 170 Mesh0.1% retained
 200 Mesh0.3% retained
 325 Mesh3.6% retained
pH 8.7
Specific Surface Area 0.90 - 1.2 m²/g
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 6.0 - 6.5
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
 
Component Elements PropertiesOriginal ValueComments
Al2O3 18.5 %
CaO 1.5 %
Fe2O3 0.060 %
H2O, Water 0.10 %
K2O 4.1 %
Loss on Ignition(%) 0.30 %
Na2O 6.5 %
SiO2 68.6 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Imerys Minspar™ 10 Ground Feldspar
Imerys Minspar™ 7 Ground Feldspar
Imerys Minspar™ 4 Ground Feldspar
Old Hickory FC-340 Tennessee Ball Clay
Old Hickory S-4 Tennessee Ball Clay

CIMERY011 / 88361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.