MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin PTFE D-310 Polytetrafluoroethylene Aqueous Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Daikin PTFE D-310 is a modified polytetrafluoroethylene aqueous dispersion manufactured without the use of PFOA. D-310 has been specifically designed for use in release coatings, cookware, and glass cloth impregnation applications where improved gloss, adhesion, surface smoothness and wear properties are desired. D-310 contains a more environmentally friendly surfactant that leaves fewer residues in the substrate than traditional surfactants.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 - 1.53 g/cc
Solids Content 56 - 61 %
pH 8.5 - 10.5
Viscosity <= 35 cP
@Temperature 25.0 °C
Thickness <= 28.0 micronsCritical Cracking Thickness
 
Descriptive Properties
AppearanceMilky White Liquid
Surfactant Content6-7.2%PTFE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
Chemours Teflon® PTFE Grade 305A Aqueous Dispersion
Daikin PTFE D-210 DISPERSION Polytetrafluoroethylene Aqueous Dispersion
Daikin POLYFLON D-1E PTFE Dispersion
Daikin NEOFLON® AP-201 PFA

PDAIJ9897 / 209968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.