POLYCOR® 948 Series enamels are formulated to be used as topcoats on fiberglass laminates such as boat and camper shell interiors. Normally enamels are used as interior finishes or to cover a laminate to provide a colored surface. POLYCOR® 948 Series enamels are available in white or any of the colors listed in the standard color gel coat color deck. Special colors are available upon request. They can be made from an isophthalic or ISO/NPG base resin. Consult a Polynt Composites sales representative to find out more about a particular product. Features and Benefits: - Cure tack-free
- Can be used like paint – a topcoat to seal and hide a substrate
- Produce a hard, tough, durable, flat finish
- Good water resistance characteristics
- Reduced VOC emissions
Information provided by Polynt Composites. |