MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its mechanical properties i.e. yield strength, are twice those of 304/316 austenitic grades. This allows the designer to save weight, particularly for properly designed pressure vessel applications. The alloy is particularly suitable for applications covering the -50°C/+300°C (-58°F/572°F) temperature range. Lower temperatures may also be considered, but need some restrictions, particularly for welded structures. With its duplex microstructure, low nickel and high chromium contents, the alloy has improved stress corrosion resistance properties compared to 304 and 316 austenitic grades.

Information provided by manufacturer.

Key Words: EURONORM 1.4362 - X2 Cr Ni 23.4, AFNOR Z3 CN 23.04 Az, DIN W. Nr 1.4362, ASTM A240 - UNS S32304
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 180 - 230180 - 230Typical
Hardness, Rockwell C <= 20<= 20Typical
Tensile Strength, Ultimate >= 600 MPa>= 87000 psi
Tensile Strength, Yield  >= 400 MPa
@Strain 0.2 %
>= 58000 psi
@Strain 0.2 %
 >= 440 MPa
@Strain 1 %
>= 63800 psi
@Strain 1 %
Elongation at Break >= 25 %>= 25 %
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.3330.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
10900 ksi
@Temperature 68.0 °F
Charpy Impact >= 90.0 J>= 66.4 ft-lb
 150 J111 ft-lbTypical
 >= 75.0 J
@Temperature -50.0 °C
>= 55.3 ft-lb
@Temperature -58.0 °F
 90.0 J
@Temperature -50.0 °C
66.4 ft-lb
@Temperature -58.0 °F
Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm
@Temperature 20.0 °C
0.0000800 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.0 µm/m-°C
@Temperature 20.0 - 100 °C
7.22 µin/in-°F
@Temperature 68.0 - 212 °F
 13.5 µm/m-°C
@Temperature 20.0 - 200 °C
7.50 µin/in-°F
@Temperature 68.0 - 392 °F
 14.0 µm/m-°C
@Temperature 20.0 - 300 °C
7.78 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.450 J/g-°C
@Temperature 20.0 °C
0.108 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K
@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 23 %23 %
Iron, Fe 72.679 %72.679 %As remainder
Molybdenum, Mo 0.20 %0.20 %
Nickel, Ni 4.0 %4.0 %
Nitrogen, N 0.10 %0.10 %
Sulfur, S 0.0010 %0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel
MetalTek MTEK 29M Cast UNS J93370 Duplex Stainless Steel
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Sandvik SAF 2205 Billet

NINDUST12 / 17550

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.