MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Metech 3610 Gold Alloy Conductor Composition
Categories: Polymer; Adhesive

Material Notes: Gold alloy conductor composition 3610 is a mixed bond composition designed for microcircuit applications requiring aluminum wire bonds. It offers excellent aged wire bond adhesion for both aluminum and gold wires. The composition fires at 850°C to a dense, pin-hole free film with a typical fired thickness of 9-11 microns. The vehicle system permits resolution of 125 micron lines and spaces.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 190000 - 240000 cP
@Temperature 25.0 °C
HBT, Spindle #SC4-14 @ 10rpm
Thickness 9.00 - 11.0 micronsFired
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.0040 ohm
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
Coverage (cm²/gm)50-60Calculated from 50 micron wet film
Line Resolution (microns)125
Wire Bond Strength (grams)13-15Ultrasonic Aluminum, Initial
 7-9Ultrasonic Aluminum, Aged (300ºC for 1 hour)
 8-10Thermosonic Gold, Aged (300ºC for 1 hour)
 9-11Thermosonic Gold, Initial

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6025 Composition Spec
516.0 Aluminum Composition Spec
Aluminum 3103B Composition Spec
Aluminum 2032 Composition Spec
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 315°C (600°F) temper, 25 mm (1 in.) round

PLORD084 / 86092

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.