MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODURE® N 100A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Desmodur N 100A is an aliphatic crosslinker (HDI biuret). It is suitable as the hardener component for lightfast polyurethane coating systems.

Properties / Applications: Desmodur N 100A is used primarily as the hardener component for lightfast two-pack polyurethane coatings with high resistance to chemicals and weathering, very good gloss retention and outstanding mechanical properties. Preferred co-reactants are polyacrylate or polyester polyols. The main applications for systems based on Desmodur N 100A are as air- and force-drying coatings for automotive and industrial finishing, for wood, furniture and plastics and for corrosion protection. As with any product, use of Desmodur N 100A in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/cc
Viscosity 5000 - 10000 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 181 °C
 
Descriptive Properties
Color<80Hazen
Content<0.7%Monomeric HDI
 20-24%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODURE® N 3300A Polyurethane
Covestro DESMODURE® N 3390A BA/SN Polyurethane
Covestro DESMODURE® N 3400 Polyurethane
Covestro DESMODURE® N 3600 Polyurethane
Covestro DESMODURE® N 3800 Polyurethane

PCOVEST0555 / 202338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.