System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Elix Polymers ELIX ABS P2MC Acrylonitrile Butadiene Styrene (ABS)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
Material Notes:
Electroplating grade
ISO Shortname: ISO 2580-1 -ABS 0, MG, 095-30-25-20
Information provided by Elix Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.03
g/cc
ISO 1183
Linear Mold Shrinkage
0.0040
-
0.0070
cm/cm
60x60x2; ISO 294-4
Linear Mold Shrinkage, Flow
0.0040
-
0.0070
cm/cm
60x60x2; ISO 294-4
Melt Flow
25
g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
90.0
MPa
ISO 2039-1
Tensile Strength, Yield
40.0
MPa
50 mm/min; ISO 527-1,-2
Elongation at Break
>= 15 %
50 mm/min; ISO 527-1,-2
Elongation at Yield
2.4 %
50 mm/min; ISO 527-1, -2
Tensile Modulus
2200
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
62.0
MPa
2 mm/min; ISO 178
Flexural Modulus
2100
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
12.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
23.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Charpy Impact Unnotched
150
kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
NB
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched
14.0
kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
24.0
kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+13
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
IEC 60093
Dielectric Constant
2.9
@Frequency 1e+6 Hz
IEC 60250
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength
37.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor
0.050
@Frequency 100 Hz
IEC 60250
0.080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
96.0
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
94.0
°C
ISO 75-1,-2
Vicat Softening Point
95.0
°C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
Glow Wire Flammability Index
700
°C
@Thickness 2.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Melt Temperature
240
°C
Injection molding; ISO 294
Mold Temperature
70.0
°C
Injection molding; ISO 294
Injection Velocity
240
mm/sec
Injection molding; ISO 294
Descriptive Properties
Burning rate
55 mm/min
US-FMVSS, ISO 3795, 2 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Elix Polymers Elix™ P2MC ABS Polymer
Edinburg Plastics AGG625 ABS
Elix Polymers ELIX ABS M305 Acrylonitrile Butadiene Styrene (ABS)
Beryllium Copper, UNS C17000, TM08 Temper Strip
INEOS Styrolution Clearblend 165 MBS
PELIX015 / 183330
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.