MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Elastollan® 2180 A TPUR
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance.

Typical Applications: Polyester/Polyether based for fibers/films.

Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°C

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183-1-A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77ISO 868
Tensile Strength 45.0 MPaISO 37
Tensile Strength, Yield 1.00 MPa20% Strain; ISO 37
Elongation at Break 450 %ISO 37
100% Modulus 0.00450 GPa
@Strain 100 %
ISO 37
300% Modulus 0.0100 GPa
@Strain 300 %
ISO 37
Charpy Impact, Notched NB
@Temperature -30.0 °C
DIN ISO 179
 NB
@Temperature 23.0 °C
DIN ISO 179
Tear Strength 40.0 kN/mDIN ISO 34-1/Bb
Abrasion 45[mm3; ISO 4649
Compression Set 14 %
@Temperature 23.0 °C
DIN EN ISO 815
 23 %
@Temperature 70.0 °C
DIN EN ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 220 °CExtrusion
Mold Temperature 20.0 - 70.0 °C
 
Descriptive Properties
Commercial StatusNorth America
Primary Processing TechniqueExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® 1154 D KFFC TPUR
BASF Elastollan® 1185 A M TPUR
BASF Elastollan® SP 9213 TPUR
BASF Elastollan® 1185 A W TPUR
BASF Elastollan® 1185 A WM TPUR

PBASG0542 / 132175

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.