System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Pfluon® 8200G PEEK
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
;
Polyetheretherketone, PEEK, Unreinforced
Material Notes:
PFLUON PEEK® has high temperature resistance, self-lubricating property, easy processing and high mechanical strength.
Data provided by the manufacturer.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.30
g/cc
0.0470
lb/in³
ISO1183
Moisture Absorption
0.0700 %
@Temperature 23.0 °C
0.0700 %
@Temperature 73.4 °F
ISO62-1
Linear Mold Shrinkage, Flow
0.010
cm/cm
0.010
in/in
ISO 294
Melt Flow
20
g/10 min
@Load 5.00 kg,
Temperature 380 °C
20
g/10 min
@Load 11.0 lb,
Temperature 716 °F
cm^3/min volume rate; ISO1133
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
87
87
ISO868
Tensile Strength
100
MPa
14500
psi
ISO527
Elongation at Yield
40 %
40 %
ISO 527
Tensile Modulus
3.70
GPa
537
ksi
ISO 527
Flexural Strength
170
MPa
24700
psi
ISO 178
Flexural Modulus
4.20
GPa
609
ksi
ISO 178
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
1.10
J/cm²
@Temperature 23.0 °C
5.23
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
@Temperature 23.0 °C
1.00e+16
ohm-cm
@Temperature 73.4 °F
IEC60093
Thermal Properties
Metric
English
Comments
CTE, linear
50.0
µm/m-°C
@Temperature <=143 °C
27.8
µin/in-°F
@Temperature <=289 °F
ISO 11359
140
µm/m-°C
@Temperature >=143 °C
77.8
µin/in-°F
@Temperature >=289 °F
ISO 11359
Thermal Conductivity
0.290
W/m-K
2.01
BTU-in/hr-ft²-°F
ISO/CD22007-4
Melting Point
343
°C
649
°F
DSC; ISO 11357
Deflection Temperature at 1.8 MPa (264 psi)
152
°C
306
°F
ISO75-f
Glass Transition Temp, Tg
143
°C
289
°F
DSC; ISO 11357
Flammability, UL94
V-0
V-0
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Pfluon® 8100G PEEK
Mitsubishi Chemical Advanced Materials Semitron™ ESd 490HR PEEK Non-sloughing and low moisture absorption
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Mitsubishi Chemical Advanced Materials Ketron™ HPV PEEK High Pressure Velocity Polyetherether Ketone
Pfluon® 8800G PEEK
PPFLUON91 / 198166
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.