MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient OnFlex™ S KE 40A-3S1727 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety polar substrates including PC, ABS, PC/ABS, ASA and PVC. OnFlex-S KE compounds can be processed by 2K molding or overmoulding, insert moulding or co-extrusion. In addition to this OnFlex-S KE compounds are formulated to provide good compression set performance, even at elevated temperatures, good processability, a wide hardness range, low temperature flexibility, good scratch resistance, good colourability and surface appearance, and excellent mechanical properties.

Properties are measured using injection molded plaques. Compression Set values are for parts annealed for 24 hours at 100°C.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40ISO 868
Tensile Strength at Break 3.60 MPaISO 37
Tensile Stress at Strain 1.20 MPa
@Strain 100 %
ISO 37
 2.80 MPa
@Strain 300 %
ISO 37
Elongation at Break 300 %ISO 37
Tear Strength 13.0 kN/mISO 34-1
Compression Set 38 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 51 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 72 %
@Temperature 100 °C,
Time 79200 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °C
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 100 °C
Dry Time 2.00 hour
 
Descriptive Properties
FeaturesGood Adhesion
 Scratch Resistant
FormsPellets
Generic MaterialTPE
Generic Material TypeStyrenic Thermoplastic Elastomer (TES)
Generic NameThermoplastic Elastomer (TPE)
Injection RateSlow-Moderate
Processing MethodCoextrusion
 Multi Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Consumer Applications
 Industrial Applications
 Overmolding
 Power/Other Tools

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ S KA 40A-3S1767 Thermoplastic Elastomer (TPE)
Avient OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE)
Avient OnFlex™ S EF 40A-3S1964 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HT 40A-3S2131 Thermoplastic Elastomer (TPE)
Avient OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE)

PH0POL1142 / 145711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.