MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Sinvicomp SIH 5005 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Availability: Asia Pacific

Features: High Heat Resistance; Good Stiffness

Uses: Electronic Insulation; Wire and Cable Applications

Wire Types: Class 1/1; Type 4; Type 5

Agency Ratings: BS 6746; UL 1581; JIS 6723

Forms: Pellets

Processing Method: Extrusion

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 93ASTM D2240
Tensile Strength, Yield 2556 psiAfter aging 240 hours at 275°F; ASTM D638
 2840 psi9.8 in/min; ASTM D638
Elongation at Break 212.5 %After Aging 240 hours at 275°F; ASTM D638
 250 %9.8 in/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 374 °F
@Time >=7200 sec
Congo Red; BS 2782

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 1-8114 SIH Crosslinker
Teknor Apex Sinvicomp SIH 5008 Polyvinyl Chloride, Flexible
Teknor Apex Sinvicomp SIH 5005A Polyvinyl Chloride, Flexible
Teknor Apex Sinvicomp SIH 7005A Polyvinyl Chloride, Flexible
Teknor Apex Sinvicomp SIH 6508A Polyvinyl Chloride, Flexible

PTEKNP167 / 129248

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.