MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite FS-5 Diallyl Meta-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

Material Notes: FS-5 is a short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound, which meets the requirements of ASTM D5948 Type SIG

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.91 g/ccASTM D782
Water Absorption 0.35 %
@Time 173000 sec
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 69.0 MPaASTM D638
Flexural Strength 110 MPaASTM D790
Flexural Modulus 11.7 GPaASTM D790
Compressive Strength 131 MPaASTM D695
Izod Impact, Notched 32.0 J/mASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength >= 14.8 kV/mm
@Frequency 60 Hz
SS, wet
Dissipation Factor 0.014
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 175 secASTM D495
Comparative Tracking Index >= 600 VTracking Resistance; ASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°CASTM E831
Thermal Conductivity 0.360 W/m-KASTM C518
Maximum Service Temperature, Air 130 °CUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °CAs Molded; ASTM D648A
Oxygen Index 29 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite 73-70-70 C-P Diallyl Ortho-Phthalate Molding Compount
Sumitomo Bakelite 52-01 Diallyl Ortho-Phthalate Molding Compound
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole
Cosmic Plastics ID-40 Orlon Filled Diallyl Iso-Phthalate Molding Compound
Cosmic Plastics E4920FC Mineral Filled Epoxy Molding Compound

PSUMIT164 / 193969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.