MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized

Processing Method: Injection Molding

Forms: Pellets

Automotive Specifications: Chrysler MS-DB41 CPN2239 Color: BK001 Black; Chrysler MS-DB41 CPN3794 Color: Non-matched Color; Chrysler MS-DB41 CPN4061 Color: 100% Color Match; Ford ESA-M4D349-A; GM GMP.PA66.020

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 16500 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Elongation at Yield 3.0 %ASTM D638
Flexural Strength 24500 psiASTM D790
Flexural Modulus 675000 psiASTM D790
Izod Impact, Notched 1.20 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Strength 460 V/mil
@Thickness 3.00 mm
ASTM D149
Comparative Tracking Index 600 VUL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 419 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.810 mm
Oxygen Index 25 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 465 - 495 °F
Middle Barrel Temperature 495 - 520 °F
Front Barrel Temperature 505 - 535 °F
Nozzle Temperature 505 - 540 °F
Melt Temperature 495 °F
 505 - 540 °FProcessing Temperature
Drying Temperature 175 °F
Moisture Content 0.20 %
 
Descriptive Properties
AppearanceBlack; Natural Color
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Teknor Apex Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced
Teknor Apex Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade

PTEKNO437 / 128614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.