MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lushan 5% WR-2 Wood Plastic Composites Compatibilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Compatibilizer/coupling agent Lushan series for wood plastic composites is a maleic anhydride grafted polyolefins, applied in PE, PVC, wood powder, and bamboo powder and wood fiber composite materials. The molecular chain of compaitbilizer contains a large number of carboxyl and anhydride-based, which can occur esterification with the hydroxyl in wood fiber, to reduce the polarity and absorbability of wood fibers. Compatiblizer/coupling agent Lushan series can make wood fibers and plastics have good compatibility, improve wood fiber’s dispersion in plastics and improve the mechanical properties of wood-plastics have good compatibility, improve wood fiber’s dispersion in plastics and improve the mechanical properties of wood-plastic composite materials.

Compatibilizer for Wood Plastic Composites Usage:

  • High maleic anhydride grafted polyethylene for compatibilizer between PE matrix resin and wood fiber
  • Suitable melt viscosity and excellent miscibility with wood fiber and other materials

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1.20 MPa
Flexural Strength 0.850 MPa
Izod Impact, Notched (ISO) 0.350 kJ/m²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lushan 2% WR-2 Wood Plastic Composites Compatibilizer
Akzo Nobel Injection molding of 20% Wood Plastic Composite with 3.25% Expancel 092-120
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound
FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound
Lushan WR-2 Wood Plastic Composites Compatibilizer

PLUSH049 / 150047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.