MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wellman Wellamid® GF1398-BK1 Nylon 66, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes:

All information provided by Wellman Engineered Resins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183-87
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cmDIS 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cmDIS 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPaISO 527-93
Elongation at Break 2.0 %ISO 527-93
Flexural Strength 225 MPaISO 178-93
Flexural Modulus 8600 MPaISO 178-93
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180-93
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75-93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass
DuPont Mobility and Materials Zytel® 70G33HSL BK083 PA66-GF33
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0

PWEL00144 / 88064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.