MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wax to improve the blend viscosity, grease resistance, blocking temperature, scuff resistance, and gloss. Epolene C-17 commonly replaces granular LLDPE as the base polymer in color concentrates because it's easier to process and has higher output rates. Epolene C-17 has good high temperature stability, low color, low temperature flexibility, and excellent compatibility with various tackifying resins.
    Key Attributes:
  • Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR
  • Excellent thermal stability
  • Low color
  • Medium molecular weight
  • Useful in color concentrates
    Application/Uses:
  • Hot Melt Adhesive
  • Packaging
  • Solvent borne Adhesives
  • Wax Modification

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 - 0.919 g/cc0.0330 - 0.0332 lb/in³ASTM D4883
Brookfield Viscosity 19 cP
@Load 0.00000220 kg,
Temperature 190 °C
19 cP
@Load 0.00000475 lb,
Temperature 374 °F
Molecular Weight 100000 g/mol100000 g/mol
Melt Flow 16 - 24 g/10 min16 - 24 g/10 minASTM D1238
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 343 °C>= 649 °FASTM E136
Ring & Ball Softening Point 133 °C271 °FASTM E28
 
Descriptive Properties
Penetration Hardness2 dmmASTM D5, Needle under 100-g load 5s @ 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF9022 / 106859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.