MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LLDPE LL 1004YB Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 1004YB is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. The grade contains a higher level of antioxidants and has excellent Environmental Stress Crack Resistance (ESCR). Sufficient Cu-inhibitor should be added to meet specific ageing requirements for insulation. For jacketing applications, addition of Carbon Black or UV stabilizer is required.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Halogen-free flame retardant (HFFR) compounds
  • LV silane cross-linkable insulation – 1 step process
  • LV silane cross-linkable insulation – 2-step process

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil method
Melt Flow 2.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 1900 psiASTM D638
Tensile Strength, Yield 1700 psiASTM D638
Elongation at Break 710 %ASTM D638
Elongation at Yield 20 %ASTM D638
Flexural Modulus, 1% Secant 36000 psiASTM D790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.80e+15 ohm-cmASTM D257
Dielectric Constant 2.2
@Frequency 60 Hz
ASMT D150
Dielectric Strength 1300 V/milASTM D149
Dissipation Factor 0.00040
@Frequency 60 Hz
ASMT D150
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 250 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LLDPE LL 1004YB Film Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil C6LL 4342.48 Linear Low Density Polyethylene Resin

PEX99184 / 175420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.