MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Edistir R 540E Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection moldings.

Designation: Thermoplastics ISO 2897-PS-I,G,093-03-07-18

Applications: To be used in industrial panels for appliances and buildings. Injection molding of shoe heels.

R 540E satisfies UL94 HB at 1.5 mm (internal test).

This grade in natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (included the EEC Directive 90/128 and following amendments).

Information provided by Polimeri Europa

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 g/ccISO 60
Density 1.04 g/ccISO 1183
Water Absorption <= 0.10 %24 hours - 23°C; ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmInternal Method
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 70ISO 2039/2
Tensile Strength at Break 29.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 24.0 MPa50 mm/min; ISO 527
Elongation at Break 60 %50 mm/min; ISO 527
Tensile Modulus 2.00 GPa1 mm/min; ISO 527
Flexural Strength 43.0 MPa2 mm/min; ISO 178
Izod Impact, Notched 100 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ISO 180/4A
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
ISO 180/1A
 8.00 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+15 ohm-cmIEC 60093
Surface Resistance 1.50e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 50 Hz
IEC 60250
Dielectric Strength 65.0 kV/mmIEC 60243
Dissipation Factor 0.00030
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 500 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM D 696
Thermal Conductivity 0.170 W/m-KISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C120°C/h; ASTM D 648
Vicat Softening Point 92.0 °C50 N - 50°C/h; ISO 306/B
 100 °C10 N - 50°C/h; ISO 306/A
Flammability, UL94 HB
@Thickness 1.50 mm
UL94
Glow Wire Test 650 °C
@Thickness 1.60 mm
IEC 60695-2-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 240 °CExtrusion
 210 - 260 °CInjection Molding
Mold Temperature 20.0 - 60.0 °CInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Edistir R 850E Polystyrene
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
Versalis Edistir N 1910 Polystyrene
Versalis Edistir N 2982 Polystyrene
Resirene Resirene® 9720 High Impact Polystyrene

PENI409 / 35846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.