MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed CHEMRAZ® 551 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: With its broad chemical resistance, Chemraz® 551 is ideally suited as a universal sealing material for aqueous semiconductor wafer processing and chemical/DI water distribution systems. Chemraz 551 provides a significantly wider operational band and superior compression set resistance than any other broad range perfluoroelastomer on the market. With an upper temperature limit of 316°C (600°F), it is the elastomer of choice for the most demanding applications from ozonated DI water to Hot Sulfuric Resist Strip.

Chemraz 551 is one of Greene Tweed’s many cost-effective products and services that increase the reliability and extend the lifetime of our customers’ equipment in challenging aqueous conditions while protecting both the operator and the environment from harmful fluid leaks.

Applications:

  • Valve seals
  • Fitting and union seals
  • Gaskets
  • Regulator seals
  • Filter seals
  • Dispensing seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 23.61 MPa3425 psiASTM D1414
Tensile Strength, Yield 3.10 MPa450 psi@50% Elongation; ASTM D1414
 10.17 MPa1475 psi@100% Elongation; ASTM D1414
Elongation at Break 175 %175 %ASTM D1414
Compression Set 20 %
@Temperature 204 °C,
Time 252000 sec
20 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 316 °C600 °F
Minimum Service Temperature, Air -12.2 °C10.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 537 Perfluoroelastomer
Greene Tweed CHEMRAZ® 534 Perfluoroelastomer
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer
Greene Tweed CHEMRAZ® 526 Perfluoroelastomer
Greene Tweed CHEMRAZ® 522 Perfluoroelastomer

PGREEN14 / 42308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.