MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alcoa 2090-T83 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has a 10 per cent higher elastic modulus. When coupled with the low density feature, this provides for unique weight saving benefits. Alloy 2090-T83 has strengths comparable with other high strength aluminum alloys and superior corrosion resistance. The alloy is also one of the most weldable aluminum products available.

Information provided by Alcoa.

Key Words: UNS A92090; Aluminium 2090-T83; AlLi; Aluminum Lithium Alloy; AA2090-T83
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.59 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 64000 psi
@Thickness 3.17 mm
45° Direction
 >= 73000 psi
@Thickness 3.17 mm
LT Direction
 >= 77000 psi
@Thickness 3.17 mm
Longitudinal Direction
Tensile Strength, Yield >= 56000 psi
@Thickness 3.17 mm
45° Direction
 >= 66000 psi
@Thickness 3.17 mm
LT Direction
 >= 70000 psi
@Thickness 3.17 mm
Longitudinal Direction
Elongation at Break >= 3.0 %
@Thickness 3.17 mm
Longitudinal Direction
 >= 5.0 %
@Thickness 3.17 mm
LT Direction
Modulus of Elasticity 11500 ksi
Fatigue Strength 15000 psi
@# of Cycles 1.00e+7
Notched (KT = 3)
 16000 psi
@# of Cycles 1.00e+6
Notched (KT = 3)
 21000 psi
@# of Cycles 100000
Notched (KT = 3)
 30000 psi
@# of Cycles 1.00e+7
Smooth
 33000 psi
@# of Cycles 10000
Notched (KT = 3)
 35000 psi
@# of Cycles 1.00e+6
Smooth
 44000 psi
@# of Cycles 100000
Smooth
 68000 psi
@# of Cycles 10000
Smooth
Fracture Toughness 40.0 ksi-in½
@Thickness 3.17 mm
KC, L-T
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
per Aluminum Association
Specific Heat Capacity 1.203 J/g-°C
@Temperature 100 °C
per Aluminum Association
Thermal Conductivity 88.0 W/m-Kper Aluminum Association
Melting Point 560 - 650 °Cper Aluminum Association
Solidus 560 °Cper Aluminum Association
Liquidus 650 °Cper Aluminum Association
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 93.2 - 95.6 %As remainder
Chromium, Cr <= 0.05 %
Copper, Cu 2.4 - 3.0 %
Iron, Fe <= 0.12 %
Lithium, Li 1.9 - 2.6 %
Magnesium, Mg <= 0.25 %
Manganese, Mn <= 0.05 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.10 %
Titanium, Ti <= 0.15 %
Zinc, Zn <= 0.10 %
Zirconium, Zr 0.08 - 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2090-T86
Aluminum 8090-T8x
Aluminum 7034-T6
Aluminum 8090-T8151
Aluminum 2090-T83

NALCOA25 / 176079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.