MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Minlon® 22C NC010 PA66-(MD+GF)38
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: 38% Mineral/Glass Reinforced Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccDAM; ISO 1183
Melt Density 1.28 g/cc
@Temperature 295 °C
Water Absorption 1.0 %
@Time 86400 sec
Immersion; DAM; Sim. to ISO 62
 5.4 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.40 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 82.0 MPa50% RH; ISO 527-1/-2
 130 MPaDAM; ISO 527-1/-2
Elongation at Break 3.5 %DAM; ISO 527-1/-2
 10 %50% RH; ISO 527-1/-2
Tensile Modulus 5000 MPa50% RH; ISO 527-1/-2
 7500 MPaDAM; ISO 527-1/-2
Flexural Modulus 5000 MPa50% RH; ISO 178
 6500 MPaDAM; ISO 178
Poissons Ratio 0.34DAM
 0.3550% RH
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1U
 40.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1U
 50.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
 50.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 45.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 3.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 3.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 4.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 2300 MPa1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 1500 MPa1000h; 50% RH; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm50% RH; IEC 62631-3-1
 1.00e+13 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 3.00e+12 ohm50% RH; IEC 62631-3-2
Dielectric Constant 4.0
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 4.0
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.0
@Frequency 100 Hz
DAM; IEC 62631-2-1
 7.0
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 39.0 kV/mm50% RH; IEC 60243-1
 40.0 kV/mmDAM; IEC 60243-1
Dissipation Factor 0.010
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.010
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.020
@Frequency 100 Hz
50% RH; IEC 62631-2-1
 0.050
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 475 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 41.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 62.0 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.10 J/g-°C
@Temperature 295 °C
Melt
Thermal Conductivity 0.250 W/m-K
@Temperature 295 °C
Melt
Melting Point 263 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 230 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 80.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.810 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 40.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 24 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 295 °COptimum, Injection
 285 - 305 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaInjection
 100 MPaInjection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,(MD+GF)38,M1GHNO2R,S14-070
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66-(MD+GF)38<ISO 11469
PolymerPA66-(MD+GF)38
Processing Hold Pressure Time (s/mm)3Injection
Regional AvailabilityAsia Pacific
 North America
 South and Central America
Resin IdentificationPA66-(MD+GF)38ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL
DuPont Mobility and Materials Minlon® 22C BK086 PA66-(MD+GF)38
Celanese Celanex® 6402R PBT, 40% Mineral / Glass Reinforced
INEOS Styrolution Lustran® 288 Acrylonitrile Butadiene Styrene (ABS)
Covestro Makrolon® 6485 Polycarbonate, Injection Grade

PDSX5248 / 197888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.