MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Attane™ 4704G LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description:
    Provides improved cling in one-sided cling applications
  • It has improved toughness and optical properties
Complies with: US FDA FCN 424; EU No 10/2011. Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA FCN 424; EU No 10/2011

Form: Pellets

Processing Method: Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD  6.87 MPa
@Thickness 0.0165 mm
997 psi
@Thickness 0.000650 in
100% in cling layer; ASTM D882
 7.58 MPa
@Thickness 0.0165 mm
1100 psi
@Thickness 0.000650 in
50% in cling layer; ASTM D882
Film Tensile Strength at Yield, TD  6.96 MPa
@Thickness 0.0165 mm
1010 psi
@Thickness 0.000650 in
100% in cling layer; ASTM D882
 7.10 MPa
@Thickness 0.0165 mm
1030 psi
@Thickness 0.000650 in
50% in cling layer; ASTM D882
Film Elongation at Break, MD  480 %
@Thickness 0.0165 mm
480 %
@Thickness 0.000650 in
100% in cling layer; ASTM D882
 490 %
@Thickness 0.0165 mm
490 %
@Thickness 0.000650 in
50% in cling layer; ASTM D882
Film Elongation at Break, TD  560 %
@Thickness 0.0165 mm
560 %
@Thickness 0.000650 in
50% in cling layer; ASTM D882
 570 %
@Thickness 0.0165 mm
570 %
@Thickness 0.000650 in
100% in cling layer; ASTM D882
1% Secant Modulus  97.2 MPa
@Thickness 0.0165 mm
14100 psi
@Thickness 0.000650 in
MD, 100% in cling layer; ASTM D882
 101 MPa
@Thickness 0.0165 mm
14600 psi
@Thickness 0.000650 in
TD, 50% in cling layer; ASTM D882
 105 MPa
@Thickness 0.0165 mm
15300 psi
@Thickness 0.000650 in
TD, 100% in cling layer; ASTM D882
 109 MPa
@Thickness 0.0165 mm
15800 psi
@Thickness 0.000650 in
MD, 50% in cling layer; ASTM D882
Elmendorf Tear Strength MD  280 g
@Thickness 0.0165 mm
280 g
@Thickness 0.000650 in
50% in cling layer; ASTM D1922
 280 g
@Thickness 0.432 mm
280 g
@Thickness 0.0170 in
100% in cling layer; ASTM D1922
Elmendorf Tear Strength TD  390 g
@Thickness 0.0165 mm
390 g
@Thickness 0.000650 in
100% in cling layer; ASTM D1922
 400 g
@Thickness 0.0165 mm
400 g
@Thickness 0.000650 in
50% in cling layer; ASTM D1922
Film Tensile Strength at Break, MD  32.3 MPa
@Thickness 0.0165 mm
4690 psi
@Thickness 0.000650 in
50% in cling layer; ASTM D882
 35.2 MPa
@Thickness 0.0165 mm
5110 psi
@Thickness 0.000650 in
100% in cling layer; ASTM D882
Film Tensile Strength at Break, TD  27.5 MPa
@Thickness 0.0165 mm
3990 psi
@Thickness 0.000650 in
50% in cling layer; ASTM D882
 27.6 MPa
@Thickness 0.0165 mm
4000 psi
@Thickness 0.000650 in
100% in cling layer; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °F
Vicat Softening Point 70.0 °C158 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze  0.65 %
@Thickness 0.0165 mm
0.65 %
@Thickness 0.000650 in
100% in cling layer; ASTM D1003
 0.88 %
@Thickness 0.0165 mm
0.88 %
@Thickness 0.000650 in
50% in cling layer; ASTM D1003
Gloss  95 %
@Thickness 0.0165 mm
95 %
@Thickness 0.000650 in
45°, 50% in cling layer; ASTM D2457
 96 %
@Thickness 0.0165 mm
96 %
@Thickness 0.000650 in
45°, 100% in cling layer; ASTM D2457
 
Descriptive Properties
Film Puncture Resistance32.1 ft-lb/in350% in cling layer, 0.65 mil
 73.8 ft-lb/in3100% in cling layer, 0.65 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF408 / 311101

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.