MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the efficiency of this strengthening dispersion, a superior combination of properties can be attained for a given application. Ferrium® C61™ was designed to provide carburized surface properties similar to conventional gear steels such as AISI 9310 and EN36C with the added benefit of an ultra high-strength core along with excellent fracture toughness. C61™ should be considered for use in applications that require high case hardness, high strength, high toughness, and thermal resistance. C61™ has very high hardenability and only requires mild quenching.

Typical Applications: Power transmission shaft, gears and other demanding applications in aerospace, energy, and racing/off-road/mission-critical vehicles and other industries where weight savings, compactness, high temperature resistance and high surface fatigue resistance are valued. The high core strength and high hardenability of Ferrium® C61™ particularly benefits structural components such as shafts with integral gearing.

Workability:
Fording: Forge at 1800-2100°F (982-1149°C)

Heat Treatment:
Normalizing: Heat uniformly to 1875°F(1024°C) and air cool..
Annealing: Heat uniformly to 1250°F(677°C), hold for 2 to 8 hours and air cool.. Hardness should be less than 327 HBW.
Carburizing and Hardening: Vacuum carburize at 1830°F (1000°C), followed by quenching in gas (1.5 Bar Nitrogen or higher) or oil medium.
Refrigerate: To obtain optimum case hardness, a refrigeration treatment at -100°F (-73°C) or lower for 1 hour is recommended. This should be performed with minimal delay after completion of the quench.
Temper: At 900°F (482°C)

Product Forms: Ferrium® C61™ is manufactured in typical ingot, bar and billet forms.

Ferrium is designed by Questek Innovations, LLC. and is manufactured by Latrobe Specialty Steel under license.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 498 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 44Distance from Quenched End 1 [in]
 44Distance from Quenched End 1 1/4 [in]
 44Distance from Quenched End 1 1/2 [in]
 44Distance from Quenched End 1 3/4 [in]
 44Distance from Quenched End 2 [in]
 44.5Distance from Quenched End 3/4 [in]
 45Distance from Quenched End 1/4 [in]
 45Distance from Quenched End 1/2 [in]
 48 - 50Typical Core Hardness
 60 - 62Typical Case Hardness
Hardness, Vickers 540
@Load 0.500 kg
Depth from Surface .070 [in]
 550
@Load 0.500 kg
Depth from Surface .045 [in]
 600
@Load 0.500 kg
Depth from Surface .029 [in]
 650
@Load 0.500 kg
Depth from Surface .02 [in]
 700
@Load 0.500 kg
Depth from Surface .014 [in]
Tensile Strength at Break >= 250000 psi
Tensile Strength, Ultimate 200 ksi
@Temperature 427 °C
 220 ksi
@Temperature 204 °C
 220 ksi
@Temperature 316 °C
 240 ksi
@Temperature 21.1 °C
Tensile Strength, Yield 175 ksi
@Temperature 427 °C
 195 ksi
@Temperature 316 °C
 200 ksi
@Temperature 204 °C
 225 ksi
@Temperature 21.1 °C
 >= 208 ksi
@Strain 0.2 %
Elongation at Break >= 13 %
 15 %
@Temperature 21.1 °C
 15 %
@Temperature 204 °C
 15 %
@Temperature 316 °C
 15 %
@Temperature 427 °C
Reduction of Area 68 %
@Temperature 21.1 °C
 68 %
@Temperature 204 °C
 68 %
@Temperature 316 °C
 68 %
@Temperature 427 °C
Fatigue Strength <= 135000 psi
@# of Cycles >=1.00e+7
 <= 150000 psi
@# of Cycles >=1.00e+7
 <= 155000 psi
@# of Cycles >=1.00e+7
 <= 160000 psi
@# of Cycles 6.30e+6
 <= 162000 psi
@# of Cycles 7.30e+6
 <= 165000 psi
@# of Cycles 130000
 <= 165000 psi
@# of Cycles 330000
 <= 165000 psi
@# of Cycles 8.00e+6
 <= 175000 psi
@# of Cycles 120000
 <= 185000 psi
@# of Cycles 80000
 <= 195000 psi
@# of Cycles 43000
Fracture Toughness 130 ksi-in½
Charpy Impact 55.0 ft-lbV-notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.54 µm/m-°C
@Temperature 24.0 - 93.0 °C
 9.59 µm/m-°C
@Temperature 24.0 - 204 °C
 10.76 µm/m-°C
@Temperature 24.0 - 316 °C
 11.09 µm/m-°C
@Temperature 24.0 - 427 °C
 11.28 µm/m-°C
@Temperature 24.0 - 538 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.15 %
Chromium, Cr 3.5 %
Cobalt, Co 18 %
Iron, Fe 67.67 %
Molybdenum, Mo 1.1 %
Nickel, Ni 9.5 %
Vanadium, V 0.080 %
 
Descriptive Properties
Cycles of Failure46100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter AerMet® 310
AISI 5120 Steel, heat treated, machined to 13.7 mm, pseudocarburized, 150°C (300°F) temper
20MnCr5 Carburizing Bearing Steel (Composition Spec)
Carpenter AerMet® 100 Aged at 875°F
Latrobe Nitralloy® N™ VAC-ARC Premium Nitriding Steel

NQUEST002 / 121070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.