MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Hytrel® HTR8341G BK320 TPC-ET  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D, Slightly Lubricated, High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 0.50 %
@Thickness 2.00 mm
0.50 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Melt Flow  0.90 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
cm³/10min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040ISO 7619-1
 37
@Time 15.0 sec
37
@Time 0.00417 hour
ISO 7619-1
Tensile Strength at Break 29.0 MPa4210 psiISO 527-1/-2
Tensile Stress at Strain  6.70 MPa
@Strain 10 %
972 psi
@Strain 10 %
ISO 527-1/-2
 11.9 MPa
@Strain 50 %
1730 psi
@Strain 50 %
ISO 527-1/-2
Elongation at Break >= 300 %>= 300 %ISO 527-1/-2
 390 %390 %ISO 527-1/-2
Tensile Modulus 0.0800 GPa11.6 ksiISO 527-1/-2
Flexural Modulus 0.0800 GPa11.6 ksiISO 178
Charpy Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eA
Tear Strength 110 kN/m628 pliparallel; ISO 34-1
 120 kN/m685 plinormal; ISO 34-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 179 µm/m-°C99.4 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 168 µm/m-°C93.3 µin/in-°FISO 11359-1/-2
Melting Point 208 °C406 °F10°C/min; ISO 11357-1/-3
Glass Transition Temp, Tg -45.0 °C-49.0 °F10°C/min; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 250 °C446 - 482 °FInjection
 240 °C464 °FInjection Optimum
Mold Temperature 40.0 - 50.0 °C104 - 122 °FInjection
 45.0 °C113 °FInjection Optimum
Drying Temperature 100 °C212 °FInjection
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.080 %0.080 %Injection
 
Descriptive Properties
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking CodeTPC-ETISO 11469
ProcessingBlow Molding
 Casting
 Coatable
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationTPC-ETISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8341C BK320 TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® 8238 TPC-ET
DuPont Mobility and Materials Hytrel® HTR8136BK TPC-ET

PDSX5214 / 197854

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.