MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Jet-Weld™ TS-230 Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly.

Sprayable/extrudable grade with long set time ideal for bonding a wide variety of plastics, including polystyrene and polyacrylic. Can bond aluminum and glass to plastic and wood. The color is white/off white. The open time is 4 minutes, and the set time is 2.5 minutes.

Information provided by 3M Adhesives Division.

Key Words: 3M Adhesives Division
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 9000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45
Tensile Strength, Ultimate 22.8 MPa
Elongation at Break 700 %
Modulus of Elasticity 0.0372 GPa
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Dow BETAMATE™ 7200 Polyurethane Prepolymer
3M Jet-Weld™ TE-015 Adhesive

PMMB27 / 53474

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.