MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling SUSTAPPO® PPO
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Extruded

Material Notes: Produced from Noryl® EN 265 resin.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Water Absorption 0.20 %ASTM D570
 0.070 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength, Yield 9400 psiASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 350000 psiASTM D638
Flexural Strength 13400 psiASTM D790
Flexural Modulus 360000 psiASTM D790
Izod Impact, Notched 3.50 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.39
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+17 ohmASTM D257
Dielectric Constant 2.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.7 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°FASTM D696
Thermal Conductivity 1.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 220 °F
Deflection Temperature at 0.46 MPa (66 psi) 289 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °FASTM D648
Flammability, UL94 V-1
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
FDA No
NSF No

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestoran® 1300 nf PPE
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
Overview of materials for Polyphenylene Ether, Molded
Covestro Bayblend® W85 HI PC ASA Blend

PROCH9052 / 232755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.