MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tipco Tipcolene® FPT 20 FR VO LTHA - UL94-V0 Flame Retardant, 20% Talc Polypropylene Homopolymer, Long Term Heat Stability
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: 20% Talc Reinforced PP Homopolymer with Long Term Heat Stability

Applications: Electrical & Appliances

Processing: Injection Molding

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ASTM D792
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Break >= 10 %>= 10 %ASTM D638
Flexural Yield Strength 44.0 MPa6380 psiASTM D790
Flexural Modulus 3.37 GPa489 ksiASTM D790
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Oxygen Index 28 %28 %ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tipco Tipcolene® FPT 20 FR VO PPC - UL94-V0 Flame Retardant, 20% Talc Polypropylene Copolymer
Tipco Tipcolene® PPC FR V0 - UL94-V0 Flame Retardant Polypropylene Copolymer
A. Schulman Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
A. Schulman Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0
Teknor Apex Synres® PP HFR005 Polypropylene

PTIP290 / 70290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.