MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Garlock 3206 Neoprene/Polyester Fabric
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polyester fabric with neoprene cover.

Diaphragm sheet is manufactured with a high-quality compound designed for long service. Reinforced with high quality, square-woven duck to provide balanced structural strength over the entire area of the diaphragm. Recommended for control valves, regulators and pumps, and weather stripping.

Information provided by Garlock Rubber Technologies

Key Words: ASTM D2000-BC-714; chloroprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1600 micronsthickness of a single ply
 
Descriptive Properties
Mullen Burst Test Rating315 psig (22 bar)one ply
 655 psig (45 bar)two ply

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
COR12V Cork/Neoprene Rubber Sheet
Denka Neoprene 671A Polychloroprene
Polychloroprene Rubber (CR)
Garlock 7986 Neoprene Sheet Rubber

PGARL992 / 157465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.