MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® G1701 H (SEP) Linear Diblock Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1701 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form identified:
Kraton G1701 HU - supplied as a powder.

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1701 H is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Packaging and Polymod; and Personal Care

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D4025
Volatiles <= 1.0 %BAM 907
Kinematic Viscosity at 100°C (212°F) 15 - 19 cSt1.7%, ENJ404; BAM 1201
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
 
Chemical PropertiesOriginal ValueComments
Diblock Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64
@Time 10.0 sec
Typical values on polymer compression molded at 350°F; ASTM D2240
Tensile Strength 2.07 MPaTypical properties of film cast from toluene solution; ASTM D412
Elongation at Break >= 100 %Typical properties of film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.03-0.2%, BAM 929
 Polystyrene34.7-38.5%, Measured on the polymer before hydrogenation, BAM 919
 Total Extractables<3.0%, BAM 1206
Styrene/Rubber Ratio37/63

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® D1163 B (SIS) Linear Block Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® G1641 H (SEBS) Linear Triblock Copolymer

PKRA9902 / 132801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.