MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Applications
The PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized products offer excellent additive homogeneity, require no transfer equipment modifications and facilitate clean and safe storage and handling. They can be used in either blown or cast film extrusion. GA 502-024 is specifically formulated with extra antioxidant for use in cast film. It contains no other additives.

Processing Techniques
GA 502 series resins exhibit excellent drawdown characteristics. Recommended conditions are 375-425°F melt temperature and a 1.5-3.0:1 blow-up ratio. Using proper techniques, these products can readily be drawn below .5 mil at optimum production rates.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Thickness 1.50 mil2:1 BUR
Melt Flow 2.0 g/10 minASTM D1238
Antiblock Level 0.000 ppm
Slip Level 0.000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 750 %ASTM D882
Film Elongation at Break, TD 800 %ASTM D882
Coefficient of Friction <= 0.20ASTM D1894
Elmendorf Tear Strength MD 170 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Dart Drop Test 120 gF50; ASTM D1709A
Film Tensile Strength at Break, MD 4900 psiASTM D882
Film Tensile Strength at Break, TD 3600 psiASTM D882
1% Secant Modulus, MD 32000 psiASTM D638
1% Secant Modulus, TD 36000 psiASTM D638
 
Optical PropertiesOriginal ValueComments
Haze 12 %ASTM D1003
Gloss 60 %ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin

PEQU0338b / 36778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.