MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
403 Stainless Steel, tempered, bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Applications: Compressor blades, turbine parts.

Key Words: UNS S40300, AMS 5611, AMS 5612, ASTM A176, ASTM A276, ASTM A314, ASTM A473, ASTM A479, ASTM A511, ASTM A580, FED QQ-S-763, MIL SPEC MIL-S-863, B.S. En. 56 B, martensitic, SAE J405 (51403), DIN 1.4024, AFNOR Z 12 C 13 M, JIS SIS 403, B.S. 420 S 29, ISO 683/13 3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 167Converted from Rockwell B hardness.
Hardness, Knoop 184Converted from Rockwell B hardness.
Hardness, Rockwell B 97
Hardness, Vickers 233Converted from Rockwell B hardness.
Tensile Strength, Ultimate 765 MPa
Tensile Strength, Yield 585 MPa
@Strain 0.2 %
Elongation at Break 23 %in 50 mm
Modulus of Elasticity 200 GPa
Poissons Ratio 0.30
Fatigue Strength 275 MPa
@Diameter 25.0 mm
tempered
 380 MPa
@Diameter 25.0 mm
Annealed
Shear Modulus 76.0 GPa
Izod Impact 102 Jtempered
 122 Jannealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000570 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 µm/m-°C
@Temperature 0.000 - 100 °C
 11.3 µm/m-°C
@Temperature 0.000 - 315 °C
 11.5 µm/m-°C
@Temperature 0.000 - 540 °C
 11.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 24.9 W/m-K
Melting Point 1480 - 1530 °C
Solidus 1480 °C
Liquidus 1530 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 12.3 %
Iron, Fe 86 %
Manganese, Mn <= 1.0 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
403 Stainless Steel, annealed, bar
304 Stainless Steel
AISI 403 12Cr STAINLESS STEEL BARS FOR TURBINE BLADES (SUS 403-B)
420 Stainless Steel
316 Stainless Steel, annealed strip

MQ403E / 12924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.