MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 515 Chloride-Free, Inorganic Acid Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Specially formulated for brass, copper, mild stainless steel and non-ferrous alloys.
  • Wide active temperature range.
  • Low organic content.
  • Completely free of zinc and chlorides.
  • High fluxing activity.
  • Residues are completely water-soluble.
Description: Superior No. 515 is a water-based, water-soluble flux with extended temperature capability that begins to clean metals at room temperature. This inorganic flux is chloride-free and reaches peak activity at 260°C/500°F. Residues are non-hygroscopic and non-corrosive and will wash-off with water. Superior No. 515 is specially formulated for soldering radiators and industrial soldering applications involving mild stainless steel, copper, and non-ferrous alloys. Since it contains no chlorides, Superior No. 515 will not discolor brass due to de-zincification, and helps make post-solder metal finishing a quicker, cleaner process.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.0455 - 1.0805 g/cc
Density 8.90 lb/gal
pH <= 1.0
 
Processing PropertiesOriginal ValueComments
Processing Temperature 105 - 315 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
FormClear Pink Liquid
ResiduesWater Soluble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX071 / 185755

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.