MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
CPT C-Flex® R70-050 Clear Biocompatible TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current United States Pharmacopoeia Class VI test requirements. C-Flex® does not contain latex rubber, polyvinyl chloride, silicone rubber, or polyurethane.

Information provided by Consolidated Polymer Technologies.

Key Words: SEBS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D 792
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
Melt Flow 0.42 g/10 minCondition E; ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 481 sec.; ASTM D 2240
Tensile Strength at Break 1146 psiASTM D 412
Elongation at Break 828 %ASTM D 412
100% Modulus 0.170 ksi
@Strain 100 %
ASTM D 412
300% Modulus 0.290 ksi
@Strain 300 %
ASTM D 412
Tear Strength 100 pliNotched, Die B; ASTM D 624
 120 pliDie C; ASTM D 624
Taber Abrasion, mg/1000 Cycles 101Federal Test Method Standard, 405
Compression Set 18 %
@Temperature 23.0 °C
ASTM D 412
 53 %
@Temperature 70.0 °C
ASTM D 412
Tensile Set 20 %at 300% elongation; ASTM D 412
 73 %at break; ASTM D 412
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -87.0 °FASTM D 746
 
Optical PropertiesOriginal ValueComments
Haze 33 %ASTM D 1033A
Transmission, Visible 89 %ASTM D 1033A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 325 - 400 °FExtrusion Temperature
Middle Barrel Temperature 300 - 425 °FInjection molding cylinder temperature
Drying Temperature 150 - 200 °FDesiccant type
Injection Pressure 300 - 1000 psi
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Sterilization methods:Steam/Autoclave, Cobalt 60, Ethylene Oxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CPT C-Flex® R70-051 Clear Biocompatible TPE
CPT C-Flex® R70-085 Clear Biocompatible TPE
CPT C-Flex® R70-026 Opaque Biocompatible TPE
CPT C-Flex® R70-046 Clear Biocompatible TPE
CPT C-Flex® R70-190 Opaque Biocompatible TPE

PCPT14 / 29109

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.