MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-3803 FST Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Description: FR-3800 FST is a halogen-free polyurethane-based foam that is compliant with fire, smoke and toxicity (FST) requirements, Ohio State University (OSU) 65/65 heat release standards for aerospace interior applications and REACH regulation. It is available in a wide range of densities, from 3 to 40 pounds per cubic foot, and sheet thickness of up to 24 inches. Custom sizes and thickness are also available. The FR-3800 FST can be thermoformed, easily machined and bonded. It withstands process temperatures up to 310° Fahrenheit, which provides a larger processing window to manufacture composite parts. This FST performance core series exhibits high strength-to-weight ratio due to its cellular and cross-linked structure. It meets the mechanical property requirements for core and structural FST applications without the high cost associated with alternative materials such as thermoplastic foams and honeycomb. With the FR-3800 FST, design and performance goals are achieved while meeting fire safety requirements.

Features:

  • Passes fire, smoke and toxicity (FST) Requirements
  • Meets OSU 65/65 heat release standards
  • Sheet thickness up to 24 inches
  • Thermoformable into simple curves
  • Shapes easily with common machining methods
  • Bonds well with composite skins
  • Withstands process temperatures up to 310° Fahrenheit
  • Resistant to water absorption
  • Resistant to most chemicals and solvents
  • Will not support fungal growth
  • No edge-closing or filling needed
Applications:
  • First-class seating pods
  • Sandwich core for aircraft interior components: Ceiling panels; Wall panels; Floor ramps; Door panels; Hard points in composite panels; Passenger cabin class dividers
  • Lightweight flyaway parts
  • Edge closeouts
  • Support/shim pieces

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0480 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9.0cut foam surface; ASTM D2240
Tensile Strength 37.0 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 40.0 psiRise Parallel to Test Span; ASTM D790 Method 1-A
 40.0 psiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
Flexural Modulus 1165 psiRise Parallel to Test Span; ASTM D790 Method 1-A
 1245 psiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
Compressive Strength 10.0 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 21.0 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 26.0 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 43.0 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 329 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 586 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 786 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 1381 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Shear Strength 0.0240 ksiRise Parallel to Specimen Width; ASTM C273
 0.0310 ksiRise Parallel to Specimen Thickness; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°F
@Temperature -45.6 - 93.3 °C
GP Method
Thermal Conductivity 0.230 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 300 °FASTM E1824
 
Descriptive Properties
Tumbling Friability (%)2220 mins at 60 rpm, ASTM C421
Water Absorption0.012 lbs/ft²ASTM D2842

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-3808 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3804 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3830 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-10108 Polyurethane Foam

PGENR016 / 186802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.