MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® CL-200YNR JN (Natural) Rotational molding crosslinkable high density polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Crosslinkable (XLPE)

Material Notes: Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, excellent stress cracking resistance to gasoline and other chemicals, outstanding impact strength at temperatures as low as -40°C

Characteristics: 100 J at 3 mm Impact Strength (-40°C); ARM Test Method, 260 J at 6 mm Impact Strength (-40°C); ARM Test Method

Applications: industrial and agricultural chemical storage tanks, small engine, snowmobile, and marine fuel tanks, seats

Information provided by Chevron Phillips Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
@Temperature 50.0 °C
Condition A; ASTM D 1693
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 18.0 MPaASTM D638 Type IV
Elongation at Break 450 %ASTM D638 Type IV
Flexural Modulus 0.690 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 124 °CASTM D1525
Brittleness Temperature <= -90.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 246 - 326 °Coven temperature for hot air machines 246-326°C, special handling required

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEVM13 / 20304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.