MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® XD03 ION Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® XD03 ION is a proprietary, high performance thermoplastic sheet specifically formulated to meet aesthetic effect for the design needs of the building and retail interiors industry. Integrally pearlescent, this sheet is perfect for use with LED lighting or on its own. Its built-in antimicrobial protection, KYDEX ION Technology™, continuously fights the growth of stain and odor causing bacteria on its surface.

KYDEX® XD03 ION: superior impact, membrane pressable thermoplastic 3D laminate with integral pearlescent color. While providing good definition, it surpasses vinyl overlays, high pressure laminates and melamine in resistance to surface and edge impact. For flat lamination and membrane pressing. Its KYDEX ION Technology™ is integral to the sheet. It will not wash or wear away and will last for the life of the product.

Suggested Application:

  • Store fixtures
  • Checkout counters
  • Exhibits and displays
  • Workstations
  • Flat laminated panels
  • Logo and trademark panels
  • Kiosks
  • Cabinetry
  • Door and drawer fasciae
  • Pedestals and stands
  • Tabletops
  • Gondolas
Features:
  • Antimicrobial protection inhibits the growth of stain and odor causing bacteria on the sheet surface
  • Antimicrobial protection is integrated into the sheet
  • Antimicrobial protection keeps the surface cleaner between cleanings
  • Membrane pressable to create seamless edges, eliminating edge banding
  • Resistant to cracking and chipping
  • Solid, integral color
  • Resistant to a wide range of chemicals
  • Inherently fire retardant, no flame retardants added to material
  • Available in P-K texture and thicknesses 0.76mm (0.030”) to 1.02mm (0.040”)

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Ball Impact Resistance>3,000 mmNEMA LD3.8
Dart Impact Resistance>1,075 mmNEMA LD3.9
Dimensional Change0.0003TD, Room Temperature; NEMA LD3.12
 0.0007MD, Room Temperature; NEMA LD3.12
 0.0026MD; NEMA LD3.11
 0.0039TD; NEMA LD3.11
Radiant Heat Resistance46 secCoil, NEMA LD3.10
 47 secStrip, NEMA LD3.10
Steiner Tunnel Flame Spread/Smoke DevelopmentClass 1/A(thicknesses 1.02mm (0.040”) or less); ASTM E84
Wear Resistance3,700 cyclesNEMA LD3.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS506 / 325246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.