MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Superwool 607 Pyro-Fold and Pyro-Stack Modules
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool Pyro-Fold modules are accordion fold blocks used for lining industrial furnaces.

Superwool Pyro-Stack modules are similar to the Pyro-Fold modules with the blanket cut and stacked edge-grain rather than continuously folded.

Superwool, CMS wools are uniquely designed from pure raw materials (Calcium-Magnesium-Silicate), and specially processed to offer excellent performance in high-temperature applications. Superwool offers an alternative to traditional solutions due to its unique properties of high refractoriness and excellent non-wetting characteristics to applications requiring direct contact with molten aluminum. These light weight wools are resistant to thermal shock, provide low thermal conductivity and low heat storage combined with their enhanced solubility in body fluids. Superwool modules are available in a variety of attachment systems that utilize 316 stainless steel yoke and support tubes to meet most installation needs.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

Features:

  • Accordion style construction or edge-grain
  • Choice of available attachment systems
  • Non-wetting to molten aluminum
  • Low biopersistence
  • Thermal stability
  • Low heat storage
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Based on patented technology
  • Applications:

  • Homogenizing furnaces
  • Process heaters
  • Ceramic kiln
  • Annealing furnace
  • Heat treating furnace
  • Thermal oxidizers
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.128 g/ccAvailable in multiple densities
     0.149 g/ccAvailable in multiple densities
     0.171 g/ccAvailable in multiple densities
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.500 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    9.3 pcf
     0.505 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    8 pcf; ASTM C201
     1.125 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    9.3 pcf; ASTM C201
     1.185 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    8 pcf; ASTM C201
     2.063 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    9.3 pcf; ASTM C201
     2.175 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    8 pcf; ASTM C201
     2.678 BTU-in/hr-ft²-°F
    @Temperature 982 °C
    9.3 pcf; ASTM C201
     2.828 BTU-in/hr-ft²-°F
    @Temperature 1000 °C
    8 pcf; ASTM C201
    Melting Point 2327 °F
    Maximum Service Temperature, Air 1832 °F
     
    Component Elements PropertiesOriginal ValueComments
    CaO 25 - 35 %
    MgO 4.0 - 7.0 %
    Other 1.0 %
    SiO2 60 - 70 %
     
    Descriptive Properties
    Alumina Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Thermal Ceramics Superwool 607 Max Pyro-Fold and Pyro-Stack Modules
    China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces
    Ascend Performance Materials Vydyne® R513H BK02 Nylon 66, 13% Glass Filled
    Ascend Performance Materials Vydyne® R513 NT Nylon 66, 13% Glass Filled
    Ascend Performance Materials Vydyne® R413H NT Impact Modified Nylon 66, Glass Filled

    CTHERM296 / 2616

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.