MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Kristalex™ F115 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Kristalex™ F115 Hydrocarbon Resin is a water-clear, color stable, low molecular weight thermoplastic hydrocarbon polymer. Based on purified 8 - 9 carbon aromatic monomers, this resin is indicated for use in plastics modification, hot melt adhesives and coatings, sealants and caulks. Kristalex™ F115 is compatible with a wide variety of oils, waxes, alkyds, plastics, and elastomers, and is soluble in many common organic solvents. In EVA-based hot melt adhesives Kristalex™ F115 is compatible with EVA grades with up to 18% vinyl acetate and is useful in formulating lowcolor adhesives with improved high temperature resistance. In styrenic block copolymer based adhesives Kristalex™ F115 preferentially associates with the styrenic endblocks, producing higher cohesion at temperatures up to 70°C without affecting tack and adhesion properties.

Application/Uses:

  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
Key Attributes:
  • Excellent thermal stability
  • High softening point
  • Made from purified aromatic monomers
  • Water-white initial colorr

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
Viscosity 400 cP
@Temperature 200 °C
Melt
 1200 cP
@Temperature 180 °C
Melt
 5500 cP
@Temperature 160 °C
Melt
 46000 cP
@Temperature 140 °C
Melt
Molecular Weight 400 g/molMz
 1900 g/molMw
 5500 g/molMn
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 117 °CASTM E 28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Color24 hours @ 177°C
 Hunterlab b, 5 cm path length

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5344 / 222538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.