MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool Waterproof Paper 1260
Categories: Ceramic; Oxide

Material Notes: Kaowool 1260 Waterproof Paper is manufactured from high purity refractory fibers and designed for high temperature insulation. Advanced production techniques ensure uniform fiber distribution and close control of thickness and density. Kaowool 1260 Waterproof Paper is produced from Alumina-Silicate fibers with the minimum addition of carefully selected bonds, which burn out cleanly in service. Kaowool 1260 Waterproof Paper exhibits excellent strength, flexibility and good handling characteristics. Other beneficial properties include low thermal conductivity, low thermal mass and exceptionally high thermal shock resistance.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.210 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.750 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0580 W/m-K
@Temperature 200 °C
BS 1902 Part 6
 0.0740 W/m-K
@Temperature 300 °C
BS 1902 Part 6
 0.0900 W/m-K
@Temperature 400 °C
BS 1902 Part 6
 0.110 W/m-K
@Temperature 500 °C
BS 1902 Part 6
 0.130 W/m-K
@Temperature 600 °C
BS 1902 Part 6
 0.195 W/m-K
@Temperature 800 °C
BS 1902 Part 6
Melting Point >= 1760 °C
Shrinkage 3.5 %
@Temperature 1260 °C,
Time 86400 sec
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 9.0 %
 
Descriptive Properties
Acoustic Absorption Coefficient0.02BS 3638, 2.00 mm thickness, 500HZ
 0.05BS 3638, 2.00 mm thickness, 100HZ
 0.07BS 3638, 2.00 mm thickness, 1000HZ
 0.26BS 3638, 2.00 mm thickness, 2000HZ
 0.5BS 3638, 2.00 mm thickness, 4000HZ
Classification Temperature (°C)1260
Colorwhite
Fiber Diameter2-3µm
Thickness measurement pressure10kPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF7051 / 203350

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.