MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Kennametal Stellite Delcrome® 90 White Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; White Cast Iron

Material Notes: Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. White cast iron, abrasion resistant. Carbide modifiers can provide a refined microstructure and improved corrosion resistance.

Processing: Anneal: 6hours/790°C (1450°F), furnace cool to HRC 35-45; Harden: 2 hours/1090°C (1980°F), air cooled to HRC 55-63. Can be milled and turned in the annealed condition if hardness is below HRC 40. Final grinding should be done on hardened piece to allow for distortion during heat treatment.

Corrosion Resistance: Generally superior to mild steel, but worse than 410 stainless steel. Significant corrosion in weak acids and will pit in the presence of chloride. Oxidation resistance up to 980°C (1800°F).

Applications: Abrasive applications below 540°C (1000°F) where corrosion is mild; pulverizer parts, pump barrel liners, cement valve slides, wear plates, and dry bearings.

Forms: Shapes using all casting processes, comparable hardfacing consumables.

Product of former Deloro Stellite Inc. Similar to Delcrome 50V

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.59 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 595 - 740
 70
@Temperature 900 °C
Hot Hardness
 164
@Temperature 700 °C
Hot Hardness
 228
@Temperature 600 °C
Hot Hardness
 338
@Temperature 500 °C
Hot Hardness
 400
@Temperature 400 °C
Hot Hardness
 540
@Temperature 20.0 °C
Hot Hardness
Hardness, Knoop 667 - 830Converted from Brinell hardness
Hardness, Rockwell C 55 - 63
Hardness, Vickers 640 - 798Converted from Brinell
Tensile Strength, Ultimate 450 MPa
Elongation at Break <= 1.0 %
Modulus of Elasticity 225 GPa
Izod Impact Unnotched 4.00 J
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.03 µm/m-°C
@Temperature 20.0 - 100 °C
 14.46 µm/m-°C
@Temperature 20.0 - 300 °C
 15.18 µm/m-°C
@Temperature 20.0 - 900 °C
 15.72 µm/m-°C
@Temperature 20.0 - 700 °C
 15.73 µm/m-°C
@Temperature 20.0 - 500 °C
Melting Point 1255 - 1308 °C
Solidus 1255 °C
Liquidus 1308 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.7 %
Chromium, Cr 27 %
Iron, Fe 67.8 %
Manganese, Mn 0.90 %
Silicon, Si 0.80 %
Vanadium, V 0.80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Delcrome® 93 White Cast Iron
Class III Type E 25% Cr Martensitic White Cast Iron
Haynes Stellite Alloy No. 27 cast, (UNS R30027) Superalloy
Stellite Alloy No. 21 cast (UNS R30021) Superalloy
Class II Type A 12% Cr Martensitic White Cast Iron

NSJNAA / 19192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.