MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elastomer Engineering E700-70 Polyurethane
Categories: Polymer; Thermoplastic; Polyester, TP; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: An extremely tough polyester-based urethane with excellent shock absorbing quality and resistance to abrasion and chemicals. Typical uses: shock deadening pads, abrasion resistant liners and pads, drive rollers, and printing rollers.

Information provided by Elastomer Engineering Inc (EEI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength, Ultimate 41.4 MPa6000 psi
Elongation at Break 500 %500 %
Tear Strength 8.77 kN/m50.0 pliD-470
 52.6 kN/m300 pliDie C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyPLASTY PolyTAN 15/80 Polyurethane
Lubrizol ESTANE® 58680 Ester Based Thermoplastic Polyurethane
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane

PELAS01 / 35673

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.