MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Adamas Lakinor® U PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 - 1.82 g/ccASTM D792
Water Absorption 0.00 - 0.015 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80ASTM D2240
Ball Indentation Hardness 90.0 - 120 MPaISO 2032
Tensile Strength at Break 35.0 - 50.0 MPaISO 527-1
Elongation at Break 20 - 40 %ISO 527-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Strength 18.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.190 W/m-KASTM C 177
Melting Point 175 °CDSC
Maximum Service Temperature, Air 150 °CDSC
Minimum Service Temperature, Air -50.0 °CDSC
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omnia Plastica Kynar® PVDF
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride - extruded products
GEHR Plastics PVDF Polyvinylidene Fluoride
Hippe PVDF
ScanTube PVDF Tubing

PHADAM062 / 147248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.